On Fri, Nov 18, 2022 at 03:03 PM, Jim Strohm wrote:
You may want to try Cool-Amp, but it's awfully expensive.
You have to ask the question, how the thickness of that plating compares the the skin thickness.
At 1 MHz, skin thickness is 0.0025". I don't have any guess for the thickness of that plating,
but I don't thing it is near 0.0025".
?I wonder if you can put more than one layer on or if the bond is only copper to silver and not silver to silver.
?????????????????????? Mikek