One of the basics is to use pool acid (hydrochloric/muriatic) and Hydrogen peroxide (drug store variety).

Mix one part of HCL to 6 (IIRC) parts of Hydrogen peroxide.

That etches well until the excess oxygen is used up, perhaps a month of just sitting around.

From there on, you need to bubble air through the mixture when etching.? Etching for me went from about 7 to 10 minutes with fresh peroxide, to about 20 to 30.? Others will be able to take this further.

Harvey


On 5/6/2022 8:23 PM, David Jones via groups.io wrote:

JimH

I'm a lurker and don't post much.? But I'd love to see a write up on how you make your Cupric Chloride solution.? This has been an interesting thread.