old 7633, 7613 CRT salvage


John Griessen
 

Is the gold on the inside of the ceramic envelope thick enough to bother sending to a gold refiner?
Seems similar to extracting platinum from catalytic converters, so I wonder?
They were from the per 1972 times when gold was laid on the pcbs thickly...

What is a good way to strip soldermask to expose the gold for acid to get at?
NaOH comes to mind but... I would not want to dissolve a bunch of lead/tin/copper, then put it on the ground...

I just want to send all that to the processor as "plated copper" + solder + FR4.