Re: Insert Holder Alloy


 

开云体育

Found a reference online to SS2541 being used for tool bit holders. Maybe check that.?

Get


From: [email protected] <[email protected]> on behalf of Mike Poore <mpoore10@...>
Sent: Thursday, April 25, 2024 1:09:21 AM
To: [email protected] <[email protected]>
Subject: Re: [SouthBendLathe] Insert Holder Alloy
?
The problem is I do not know the alloy. I guess I will use the 4140 specs.

On 4/25/2024 12:59 AM, Andrei via groups.io wrote:
That is definitely a great option. I don't have one so my go-to was carbide and coolant.youbare in great shape with the oven

Get

From: [email protected] <[email protected]> on behalf of Mike Poore <mpoore10@...>
Sent: Thursday, April 25, 2024 12:57:57 AM
To: [email protected] <[email protected]>
Subject: Re: [SouthBendLathe] Insert Holder Alloy
?
I have a heat treating oven right next to my mill, so I would rather use the oven.

On 4/24/2024 11:02 PM, Andrei via groups.io wrote:
Are short of squirter bottles or endmills?

Get

From: [email protected] <[email protected]> on behalf of Mike Poore <mpoore10@...>
Sent: Wednesday, April 24, 2024 10:38:03 PM
To: [email protected] <[email protected]>
Subject: Re: [SouthBendLathe] Insert Holder Alloy
?
Not an option for me.

On 4/24/2024 9:43 PM, Andrei via groups.io wrote:
Use a carbide endmill and coolant. No need to anneal

Get

From: [email protected] <[email protected]> on behalf of Mike Poore <mpoore10@...>
Sent: Wednesday, April 24, 2024 9:41:39 PM
To: [email protected] <[email protected]>
Subject: [SouthBendLathe] Insert Holder Alloy
?
Anyone happen to know the alloy most likely to be used for carbide insert tool holders? My guess is 4140. I have four that I need to mill down to work in an AXA holder. They test at 45 HRC. Thinking about annealing them before milling and then heat treating again, so I would like specs to use.