That is definitely a great option. I don't have one so my go-to was carbide and coolant.youbare in great shape with the oven
toggle quoted message
Show quoted text
I have a heat treating oven right next to my mill, so I would rather use the oven.
On 4/24/2024 11:02 PM, Andrei via groups.io wrote:
Are short of squirter bottles or endmills?
Not an option for me.
On 4/24/2024 9:43 PM, Andrei via groups.io wrote:
Use a carbide endmill and coolant. No need to anneal
Anyone happen to know the alloy most likely to be used for carbide insert tool holders? My guess is 4140. I have four that I need to mill down to work in an AXA holder. They test at 45 HRC. Thinking about annealing them before milling and then heat treating
again, so I would like specs to use.