Use a carbide endmill and coolant. No need to anneal
toggle quoted message
Show quoted text
Anyone happen to know the alloy most likely to be used for carbide insert tool holders? My guess is 4140. I have four that I need to mill down to work in an AXA holder. They test at 45 HRC. Thinking about annealing them before milling and then heat treating
again, so I would like specs to use.