Hi Snapdiode,
There is a slim chance it might be Teflon which is white and almost
impossible to glue. One way to tell if it is Teflon is that it will feel
extremely slippery to the touch. Another way to tell is that Teflon has a
very high heat resistance. If you hold a soldering iron to it nothing
happens.

Dennis Tillman W7PF

-----Original Message-----
Sent: Monday, March 21, 2016 6:25 PM
Subject: [TekScopes] Those funny 311-0603-00 pots

I thought the white part is made of Delrin, but so far it has shrugged off
every glue and solvent I threw at it.
MEK, dichloromethane, hot glue, cyanoacrylate, plastic bonder epoxy,
nothing affects or sticks to it.

How can I be sure the material is Delrin, and not say, Nylon?
------------------------------------